AQUASHUTTER
Waterproof Flexible Cement Membrane
Description

Product Details
ACG Emulsion – Emulsion for waterproofing:
ACG emulsion is a durable acrylic emulsion and used as waterproofing agent ( ACG material) after mixing with ACG admixture.
- Packing content 18 kg/PP can.
- Appearance: Milky white liquid.
ACG Admixture – Admixture for Waterproofing:
ACG admixture is a alumina cement based admixture and use as waterproofing agent (ACG material) mixing with ACG emulsion.
- Packing Content: 15kg/ bag
- Appearance: Gray powde
Properties
The material is similar to a Urethane coating, which is less susceptible to UV rays or hydrolysis.
In particular, Aquashutter has been highly weather-resistant, flexible elasticity, and waterproofing during a long period.
The product can be applied in waterproofing water tanks, underground interior, underground exterior, toilet, bathroom, kitchen, bathroom, trench pits, elevator pit.
Durability Test
Technical report
Elongation | % | 145 |
Zero span tension elongation | mm | 3.9 |
Adhesion strength (dry) | N/mm2 | 0.8 |
Water Permeability | gram | 0.1 |
Test condition | temperature | 20±2℃ |
Humidity: | 65±5% | |
Test method: Architectural Institute of Japan (Polymer-modified cement waterproofing membrane coating |
Application method
1. Priming Paint:
- Use ACG emulsion diluted 5 times in water. Blending ratio (weight ratio): ACG emulsion: water = 1:4
- Primer with 0.2kg/m2 uniformly using a paint roller
2. Mixing Instruction:
Mixing ratio ACG emulsion: ACG admixture= 18: 30 [15 × 2 bags].
- Place the pure ACG Emulsion into the vessel.
- Combine the ACG mixture with manual mixer.
- Add two bags of ACG admixture to the above mixture.
- After 3 minutes of mixing, inspect to make sure there are no lumps.
Batching Process
3. Waterproof Coating (ACG material) – First Coat, Top Coat
- Use a steel trout to apply the waterproofing coat to the surface and then smooth the coated sealant. Note: Use hand force when handling to help the waterproof layer increase adhesion.
- The quantity of paint used in construction is 1.2 kg / m2 (once only).
After making sure it has hardened so that it does not leave fingerprints when pressed, apply a second coat. hai.
- Verify that the pinhole on the first coat is dry before applying the second coat..
- In case of pinhole appearance, fill with ACG material and proceed with the second coat until there is no pinhole of the first coat.
4. Maintenance:
- Use a fan or similar device to adequately ventilate the waterproofing surface to prevent condensation.
- If rain is forecast, construction must be shut down. If the waterproof coat is washed out by rain after application, the coating must be redone.
DOCUMENTS DOWNLOAD